This search combines search strings from the content search (i.e. "Full Text", "Author", "Title", "Abstract", or "Keywords") with "Article Type" and "Publication Date Range" using the AND operator.
Beilstein J. Nanotechnol. 2014, 5, 1419–1431, doi:10.3762/bjnano.5.154
Figure 1: Bright-field TEM images of Au–TiO2 nanocomposite thin films with different MVFs, (a) 7%, (b) 11%, (...
Figure 2: Bright field TEM morphologies of Ag–TiO2 nanocomposite films with different metal volume filling fr...
Figure 3: Morphological evolutions in Au–TiO2 nanocomposite (MVF ≈ 15%) under 100 MeV Ag8+ ion irradiation at...
Figure 4: Morphological evolutions in Ag–TiO2 nanocomposite films (MVF ≈ 15%) under 100 MeV Ag8+ ion irradiat...
Figure 5: Microstructural changes in the TiO2 matrix of the nanocomposite film with MVF (Ag) ≈ 15% induced by...
Figure 6: UV–visible absorption and transmission spectra of Au–TiO2 nanocomposite films (with an MVF of about...
Figure 7: (a, b) UV–visible absorption spectra of Ag–TiO2 nanocomposite films (MVF ca. 13% and 27%, respectiv...
Figure 8: Micron-sized single crystalline TiO with the corresponding experimental SAED pattern and simulated ...
Figure 9: TEM nanoprobe EDX analysis on the TiO crystal and the matrix confirming the ratio of Ti:O in both t...
Figure 10: In situ heating of the Ag–TiO2 nanocomposites at (a) room temperature (b) 150 °C, (c) 300 °C, (d) 4...
Beilstein J. Nanotechnol. 2013, 4, 705–713, doi:10.3762/bjnano.4.80
Figure 1: Cycling behavior of C(FeF2)0.55, C(FeF2)0.55_200, C(FeF2)0.55_300 and C(FeF2)0.55_400. The material...
Figure 2: XRD pattern (Mo Kα) of: a) Nanocomposites with different C/F ratio, b) CFx precursors. *:FeF2; §:C ...
Figure 3: Measured Raman spectra and G-mode shifts of the different nanocomposites.
Figure 4: C K-edge EEL spectra of compounds with different carbon contents.
Figure 5: EEL spectra of C(FeF2)0.25_300. The spectrum shows the F K-edge and the Fe L3- and Fe L2-edges.
Figure 6: TEM and SAED pictures of a) C(FeF2)0.5_300, b) C(FeF2)0.35_300, c) C(FeF2)0.25_300 and d) one compl...
Figure 7: Discharge capacities at: a) 25 °C, b) 40 °C. The samples were cycled with a current density of 25 m...
Figure 8: Charge/discharge profiles for the first 20 cycles of the nanocomposites at 25 °C. The samples were ...
Figure 9: Long time cycling of C(FeF2)0.25_300. a) Specific discharge capacity at different temperatures, b) ...